Dimensi pengikat

nut size F E T
Lebar
Di seberang
Flat
Lebar
Di seberang
Sudut

daripada
Kacang
Saiz kacang maks. min. min. maks. min.
M1.6 0.35 3.20 3.02 3.41 1.30 1.05
M2 0.4 4.00 3.82 4.32 1.60 1.35
M2.5 0.45 5.00 4.82 5.45 2.00 1.75
M3 0.5 5.50 5.32 6.01 2.40 2.15
M3.5* 0.6 6.00 5.82 6.58 2.80 2.55
M4 0.7 7.00 6.78 7.66 3.2 2.9
M5 0.8 8.00 7.78 8.79 4.7 4.4
M6 1 10.00 9.78 11.05 5.2 4.9
M8 1.25 13.00 12.73 14.38 6.80 6.44
M10 1.5 16.00 15.73 17.77 8.40 8.04
M12 1.75 18.00 17.73 20.03 10.80 10.37
M14* 2 21.00 20.67 23.36 12.8 12.1
M16 2 24.00 23.67 26.75 14.8 14.1
M18* 2.5 27.00 26.16 29.56 15.8 15.1
M20 2.5 30.00 29.16 32.95 18.0 16.9
M22* 2.5 34 33 37.29 19.4 18.1
M24 3 36 35 39.55 21.5 20.2
M27* 3 41 40 45.2 23.8 22.5
M30 3.5 46 45 50.85 25.6 24.3
M33* 3.5 50 49 55.37 28.7 27.4
M36 4 55.0 53.8 60.79 31.0 29.4
M39* 4 60.0 58.8 66.44 33.4 31.8
M42 4.5 65.0 63.1 71.3 34.0 32.4
M45* 4.5 70.0 68.1 76.95 36.0 34.4
M48 5 75.0 73.1 82.6 38.0 36.4
M52* 5 80.0 78.1 88.25 42.0 40.4
M56 5.5 85.0 82.8 93.56 45.0 43.4
M60* 5.5 90.0 87.8 99.21 48.0 46.4
M64 6 95.0 92.8 104.86 51.0 49.1