inconel Carta Berat Helaian Dan Plat 600

Ketebalan Plat (mm)Berat (kg/m)kg/meter (lebar 1200mm)kg/meter (lebar 1500mm)kg/meter (lebar 1800mm)kg/meter (lebar 2400mm)
323.5528.335.342.456.5
431.437.747.156.575.4
539.2547.158.970.794.2
647.156.570.784.8113
862.875.494.2113150.7
1078.594118141188
1294.2113141170226
16125.6151188226301
20157188236283377
22172.7207259311415
25196.25236294353471
28219.8264330396528
32251.2301377452603
36282.6339424509678
40314377471565754
45353.25424530636848
50392.5471589707942
55431.755186487771036
604715657078481130
655106127659181224
70549.56598249891319
75588.7570788310601413
8062875494211301507
90706.5848106012721696
100785942117814131884

 

Uns N06600 Ketebalan dan Berat Helaian – Unit Imperial

Ketebalan Saiz Nominal (inci)Berat (lb/ft2)
3/167.65
1/410.2
5/1612.8
3/815.3
7/1617.9
1/220.4
9/1622.9
5/825.5
11/1628.1
3/430.6
13/1633.2
7/835.7
140.8
1 1/845.9
1 1/451.0
1 3/856.1
1 1/261.2
1 5/866.3
1 3/471.4
1 7/876.5
281.6
2 1/886.7
2 1/491.8
2 1/2102
2 3/4112
3122
3 1/4133
3 1/2143
3 3/4153
4163
4 1/4173
4 1/2184
5204
5 1/2224
6245
6 1/2265
7286
7 1/2306
8326
9367
10408

 

Ketebalan dan Berat Plat Aloi 600 – Unit Metrik

Ketebalan Plat (mm)Berat (kg/m2)
1.612.6
2.015.7
2.519.6
323.6
3.225.1
431.4
539.3
647.1
862.8
1078.5
12.598.1
15118
20157
22.5177
25196
30236
32251
35275
40314
45353
50393
55432
60471
65510
70550
75589
80628
90707
100785
110864
120942
1301051
1501178
1601256
1801413
2001570
2501963

 