Inconel 600 ketebalan kepingan logam (mm), Tiada. 14 ketebalan plat keluli, Tiada. 18 ketebalan plat keluli, Nikel 600 ketebalan plat keluli (mm).
Carta Ketebalan Helaian
| Tolok (ga) | Ketebalan Keluli (dalam.) | Ketebalan Keluli (mm) | Ketebalan Aluminium (dalam.) | Ketebalan Aluminium (mm) |
|---|---|---|---|---|
| 3 | 0.2391 | 6.07 | 0.2294 | 5.83 |
| 4 | 0.2242 | 5.69 | 0.2043 | 5.19 |
| 5 | 0.2092 | 5.31 | 0.1819 | 4.62 |
| 6 | 0.1943 | 4.94 | 0.162 | 4.11 |
| 7 | 0.1793 | 4.55 | 0.1443 | 3.67 |
| 8 | 0.1644 | 4.18 | 0.1285 | 3.26 |
| 9 | 0.1495 | 3.80 | 0.1144 | 2.91 |
| 10 | 0.1345 | 3.42 | 0.1019 | 2.59 |
| 11 | 0.1196 | 3.04 | 0.0907 | 2.30 |
| 12 | 0.1046 | 2.66 | 0.0808 | 2.05 |
| 13 | 0.0897 | 2.28 | 0.072 | 1.83 |
| 14 | 0.0747 | 1.90 | 0.0641 | 1.63 |
| 15 | 0.0673 | 1.71 | 0.0571 | 1.45 |
| 16 | 0.0598 | 1.52 | 0.0508 | 1.29 |
| 17 | 0.0538 | 1.37 | 0.0453 | 1.15 |
| 18 | 0.0478 | 1.21 | 0.0403 | 1.02 |
| 19 | 0.0418 | 1.06 | 0.0359 | 0.91 |
| 20 | 0.0359 | 0.91 | 0.032 | 0.81 |
| 21 | 0.0329 | 0.84 | 0.0285 | 0.72 |
| 22 | 0.0299 | 0.76 | 0.0253 | 0.64 |
| 23 | 0.0269 | 0.68 | 0.0226 | 0.57 |
| 24 | 0.0239 | 0.61 | 0.0201 | 0.51 |
| 25 | 0.0209 | 0.53 | 0.0179 | 0.45 |
| 26 | 0.0179 | 0.45 | 0.0159 | 0.40 |
| 27 | 0.0164 | 0.42 | 0.0142 | 0.36 |
| 28 | 0.0149 | 0.38 | 0.0126 | 0.32 |
| 29 | 0.0135 | 0.34 | 0.0113 | 0.29 |
| 30 | 0.012 | 0.30 | 0.01 | 0.25 |
| 31 | 0.0105 | 0.27 | 0.0089 | 0.23 |
| 32 | 0.0097 | 0.25 | 0.008 | 0.20 |
| 33 | 0.009 | 0.23 | 0.0071 | 0.18 |
| 34 | 0.0082 | 0.21 | 0.0063 | 0.16 |
| 35 | 0.0075 | 0.19 | 0.0056 | 0.14 |
| 36 | 0.0067 | 0.17 | – | – |
Gnee Steel juga membekalkan produk Inconel 600 tersuai dalam pelbagai saiz dan spesifikasi. Sila hantar lukisan anda kepada kami untuk sebut harga!