Feb 04, 2026 Tinggalkan pesanan

Jadual maklumat saiz kelengkapan paip Inconel 601

Dimensi kelengkapan paip Inconel 601

ASME b16.9 Kelengkapan
Saiz Paip Biasa
ANSI b16 9 Pemasangan Paip O
D Y
dinding Ketebalan T
(Sc. Siku Paip)
LR 45 Deg SikuPusat ke MukaB SR 45 Deg Siku
Berat badan
Siku LR 90 DegPusat ke MukaA Siku LR 90 Deg Berat Di Bawah SR 90 Deg SikuPusat ke MukaA SR 90 Deg Siku Berat Di Bawah
milimeter inci. milimeter milimeter Jadual milimeter kilogram milimeter kilogram milimeter kilogram
15 1/2" 21.3 2.78 STD 15.9 0.04 38.1 0.08
      3.73 X.S 15.9 0.05 38.1 0.10
20 3/4" 26.7 2.87 STD 11.1 0.04 28.6 0.08
      3.91 X.S 11.1 0.05 28.6 0.11
25 1" 33.4 3.38 STD 22.2 0.09 38.1 0.15 25.4 0.11
      4.55 X.S 22.2 0.11 38.1 0.19 25.4 0.14
32 11/4" 42.2 3.56 STD 25.4 0.14 47.6 0.28 31.75 0.18
      4.85 X.S 25.4 0.2 47.6 0.39 31.75 0.24
40 11/2" 48.3 3.68 STD 28.6 0.2 57.1 0.4 38.1 0.26
      5.08 X.S 28.6 0.25 57.1 0.5 38.1 0.35
50 2" 60.3 3.91 STD 34.9 0.36 76.2 0.72 50.8 0.5
      5.54 X.S 34.9 0.5 76.2 1.0 50.8 0.68
65 21/2" 73.0 5.16 STD 44.4 0.73 95.2 1.46 63.5 0.95
      7.01 X.S 44.4 0.91 95.2 1.82 63.5 1.27
80 3" 88.9 5.49 STD 50.8 1.1 114.3 2.18 76.2 1.45
      7.62 X.S 50.8 1.45 114.3 2.86 76.2 1.95
100 4" 114.3 6.02 STD 63.5 2.1 152.4 4.2 101.6 2.8
      8.56 X.S 63.5 2.9 152.4 5.7 101.6 3.9
125 5" 141.3 6.65 STD 79.4 3.4 190.0 6.8 127.0 4.8
      9.5 X.S 79.4 5.0 190.0 10.0 127.0 6.5
150 6" 168.3 7.11 STD 95.2 5.1 229.0 10.1 152.4 6.8
      10.97 X.S 95.2 7.7 229.0 15.3 152.4 10.2
200 8" 219.1 8.18 STD 127.0 10.2 305.0 20.4 203.0 13.6
      12.7 X.S 127.0 15.5 305.0 30.9 203.0 20.9
250 10" 273.9 9.27 STD 159.0 18.1 381.0 36.1 254.0 24.1
      12.7 X.S 159.0 24.4 381.0 48.8 254.0 32.5
300 12" 323.9 9.52 STD 190.0 26.6 457.0 53.1 305.0 35.4
      12.7 X.S 190.0 35.0 457.0 70.0 305.0 46.7
350 14" 355.6 9.52 STD 222.0 34.1 533.0 68.1 356.0 45.4
      12.7 X.S 222.0 45.0 533.0 90.0 356.0 60.0
400 16" 406.4 9.52 STD 254.0 45.0 610.0 89.3 406.0 59.5
      12.7 X.S 254.0 59.0 610.0 118.0 406.0 78.7
450 18" 457.0 9.52 STD 286.0 56.5 686.0 113.0 457.0 75.6
      12.7 X.S 286.0 75.0 686.0 150.0 457.0 100.0
500 20" 508.0 9.52 STD 318.0 85.0 762.0 140.0 508.0 93.5
      12.7 X.S 318.0 112.5 762.0 186.0 508.0 124.0
600 24" 610.00 9.52 STD 381.0 101.5 914.0 203.0 610.0 135.0
      12.7 X.S 381.0 134.5 914.0 269.0 610.0 179.0