Apr 02, 2024 Tinggalkan pesanan

ASTM A182 F53 Pusingan Bar

GNEE Steel is a prominent supplier of ASTM A182 GR F53 Round Bars, a super duplex stainless steel with a 50:50 austenite and ferrite microstructure. Also, these Super Duplex DIN 1.4410 Round Bars provide excellent corrosion resistance and strength. Super Duplex SAF 2507 Round Bars have 25 percent chromium, 4 percent molybdenum, and 7 percent nickel. This high molybdenum, chromium, and nitrogen content results in excellent resistance to chloride pitting and crevice corrosion attack. The duplex structure provides Super Duplex 2507 Round Bars with exceptional chloride stress corrosion cracking resistance. Super Duplex UNS S32750 Round Bars have better thermal conductivity and a lower coefficient of thermal expansion than austenitic stainless steels. These Super Duplex F53 Round Bars are often used in offshore platforms, heat exchangers, process and service water systems, fire-fighting systems, and injection and ballast water systems. Buy ASTM A182 F53 Bars at an affordable price from us.

stainless steel round rodstainless-steel-round

ASTM A182 F53 Super Duplex Steel Stainless Steel Bars Specification :

: ASTM, ASME
Ketebalan : 0.5mm to 500mm Diameter
Panjang : 100 to 6000mm panjang
Selesai : Terang, Poland & Hitam
Keadaan : Sejuk Dilukis & Digilap Sejuk Dilukis, Centreless Ground & Digilap
Borang : Round, Square, Hex (A/F), Rectangle, Wire (Coil Form), Wire-mesh, Billet, Ingot, Forging Etc.

 

ASTM A182 Super Duplex F53 Stainless Bar Setaraf Gred

STANDARD WERKSTOFF NR.
ASTM A182 F53 S32750 1.4410

 

UNS S32750 Super Duplex Steel SS Round Bars Chemical Composition

C P S SI CR NI MO N
0.03 max 1.2 Max 0.035 Max 0.015 Max 0.8 Max 24 - 26 6 - 3 - 0.3

 

Super Duplex WERKSTOFF NR. 1.4410 Tahan karat Rods Mekanikal Properties

Tegang Kekuatan (ksi) min Pemanjangan (% in 50mm) min Hasil Kekuatan 0.2% Proof (ksi) min Kekerasan
110 15 80 28 max

 

ASTM A182 F53 Round Bars

ASTM A182 F53 Pusingan Bar

Super Duplex Steel ASTM A182 F53 Bars

Super Duplex Steel ASTM A182 F53 Bar