Stainless Steel Checker Plate ,also called Stainless Steel Diamond Plate, is embossed on the stainless steel plate through mechanical equipment, so that the surface of the plate appears with concave and convex patterns. In the early 1960s, large-scale steel rolling mills in Europe began to produce small batches. Later, due to the excellent corrosion resistance and anti-slip properties of stainless steel pattern plates, they were adopted by many industries and became popular. The earliest pattern pattern of stainless steel checkered plates was staggered horizontal and vertical stripes, which were produced by Shanxi Taigang and Shanghai Baosteel Group in China. In the following 20-30 years, researchers made continuous experiments and improvements to achieve better anti-slip properties. The pattern design was also mass-produced, promoted and applied. In recent years, the uses of stainless steel pattern plates have been constantly innovating, breaking through, and changing. The applicable industries and product models are also constantly increasing, and product updates are becoming more frequent.

Checker Plate are divided into two categories:
The first type is rolled by a rolling mill when the steel plant produces stainless steel. The main ketebalan of this type of product is about 3-6mm, and it is in a state of annealing and pickling after hot rolling. The process is as follows:
Tahan karat keluli billet → black coil rolled by hot tandem rolling mill → thermal annealing and pickling line → tempering machine, tension leveler, polishing line → cross-cutting line → hot-rolled stainless steel pattern plate
Ini type of pattern board is flat on one side and patterned on the other. This type of pattern plate is more commonly used in chemical industry, railway vehicles, platforms and other occasions that require strength. Such products are mainly imported, generally from Japan and Belgium. Domestic products produced by Taiyuan Steel and Baosteel fall into this category.


The second category is processing companies on the market, which purchase hot-rolled or cold-rolled stainless steel plates from steel mills and mechanically stamp them into patterned plates. This type of product has one side concave and one side convex, and is often used for general civilian decoration. This type of product is mostly cold-rolled, and most of the 2B/BA cold-rolled Stainless Steel Patterned Plate on the market are of this Jenis.

304 Stainless Steel Floor Plate,ASTM 304 Stainless Steel Skid Plate Pattern Embossed Sheet,ASTM 316 316L 310S 409L SS Checker sheet,ASTM A240 304 SS Chequered Plate,1.4401 and 1.4404 Stainless Steel Floor Plate Checker Plate ,etc. GNEE Steel is your stainless steel expert, proprovideing the highest quality SS checkered plates.